quantum-sensor-probes-early-hydration-dynamics-in-terbium-doped-strontium-aluminate-cement
Quantum Sensor Probes Early Hydration Dynamics in Terbium-Doped Strontium Aluminate Cement

Quantum Sensor Probes Early Hydration Dynamics in Terbium-Doped Strontium Aluminate Cement

Materials scientists have demonstrated a quantum sensing methodology that traces the early hydration dynamics of cement binders at the individual grain scale by coupling rare-earth luminescence to defect centers in nanodiamonds. The study, reported in Archives of Civil and Mechanical Engineering, investigates terbium-doped strontium monoaluminate alongside commercial ordinary Portland cement to clarify the chemical and physical transformations occurring during the first hours of water exposure. By exploiting luminescence emitted directly from trivalent terbium ions embedded in the strontium aluminate host lattice, the research team optically pumped negatively charged nitrogen-vacancy centers in adjacent nanodiamonds. This configuration enabled direct optically detected magnetic resonance and time-resolved spin relaxometry, yielding real-time, grain-localized measurements of temperature changes, ionic release, and phase evolution that are typically obscured in conventional macroscopic analyses.

Strontium monoaluminate is a technologically prominent member of the alkaline earth aluminate family that has attracted substantial interest for high-temperature hydraulic binders and aerospace infrastructure. The compound exhibits notable physicochemical robustness, visible to infrared transparency, persistent luminescence when activated with rare-earth dopants, and a dense atomic framework capable of attenuating high-energy gamma radiation. These attributes position strontium aluminate materials as promising candidates for passive visual marking, structural components, and radiation shields in spacecraft and extraterrestrial habitats. However, developing predictable binders from strontium aluminate requires a precise mechanistic understanding of its early hydration pathway, during which rapid dissolution and nanoscale precipitation produce rapid compressive strength development within hours of mixing. Previous characterization efforts have relied on bulk techniques that average structural signals across heterogeneous paste volumes, leaving the microscopic kinetics of ion dissolution and hydrate precipitation incompletely resolved.

To overcome these observational constraints, the researchers developed direct optically detected magnetic resonance, designated as dODMR, which relies on the quantum spin states of nitrogen-vacancy color centers hosted in diamond nanoparticles. A nitrogen-vacancy defect consists of a substitutional nitrogen atom located adjacent to a vacancy in the diamond crystal lattice, possessing a ground-state electronic configuration with spin-triplet character and trigonal symmetry. Under optical excitation, the defect polarizes preferentially into its bright spin substate, while resonant microwave radiation drives transitions between spin sublevels, causing a measurable drop in optical emission. Because the zero-field splitting parameter of the defect changes predictably with ambient thermal expansion and contraction at an established sensitivity of approximately 74 kilohertz per Kelvin, nitrogen-vacancy centers function as nanoscale thermometers. In addition, when positioned within nanometers of a reacting surface, the longitudinal spin relaxation rate of the defect responds sensitively to fluctuating local magnetic and electric fields generated by surrounding ions and paramagnetic species.

Implementing direct optically detected magnetic resonance required fabricating a specialized luminescent clinker and establishing an intimate interface with nanodiamond probes. The authors prepared strontium monoaluminate powder through a two-step solid-state reaction, calcining stoichiometric proportions of strontium carbonate and aluminum oxide at 1300 degrees Celsius before milling the intermediate product and incorporating 0.04 mole percent terbium oxide. The blended formulation was pressed into pellets at 80 megapascals and sintered at 1500 degrees Celsius in air, forming monoclinic strontium monoaluminate within space group P21 without detectable secondary crystalline impurities. The sintered material was ground into a powder displaying a unimodal particle size distribution with a median diameter of 6.6 micrometers and a specific surface area of 18.13 square meters per gram. Commercial ordinary Portland cement powder displayed a coarser median particle size of 10.7 micrometers and a specific surface area of 0.61 square meters per gram. The sensing medium comprised commercial nanodiamonds measuring approximately 140 to 150 nanometers in diameter suspended in water at one milligram per milliliter, which was mixed with dry cement at a water-to-cement ratio of 0.5.

The optical excitation pathway represents the primary operational distinction between direct and conventional optically detected magnetic resonance configurations. In standard setups, nitrogen-vacancy centers are excited by an external green laser operating at 532 nanometers. In the direct scheme applied to the terbium-doped binder, continuous blue laser illumination at 405 nanometers was directed through a high-numerical-aperture oil objective onto the surface of fresh cement paste sealed inside a 0.16-millimeter-thick microchannel slide. Photons at 405 nanometers exceed the diamond defect ionization threshold and cannot pump nitrogen-vacancy centers directly. Instead, the incident blue light selectively excites trivalent terbium ions residing within the strontium aluminate crystal lattice, causing them to emit characteristic green photoluminescence peaking near 545 nanometers through radiative relaxation. This in-situ green emission optically pumps the nitrogen-vacancy centers within adjacent nanodiamonds through non-radiative energy transfer, initiating the red fluorescence cycle between 637 and 800 nanometers that permits localized magnetic resonance measurements without relying on direct external green laser excitation of the diamond particles.

Microstructural examination of the unhydrated and hydrating clinkers by scanning electron microscopy and energy-dispersive X-ray spectroscopy confirmed the uniform dispersion of dopants and sensor particles. Electron micrographs of the dry synthesized clinker revealed a dense, homogeneous morphology containing both coarse and fine grains interspersed with microscale pores, with elemental mapping demonstrating that strontium, aluminum, oxygen, and terbium were distributed uniformly across the crystal lattice. Upon exposure to water, partial hydration initiated at the grain perimeters and proceeded inward, leaving unreacted anhydrous cores surrounded by developing hydrate layers and microcracks. Energy-dispersive elemental mapping of pastes cured for up to seven days confirmed that nanodiamonds, tracked via localized carbon distributions, remained evenly embedded across the hydrating matrix rather than segregating into localized agglomerates, thereby ensuring direct contact with the evolving solid-liquid interface throughout the curing period.

Complementary X-ray diffraction and solid-state nuclear magnetic resonance analyses tracked the phase transformations that accompanied the spectroscopic measurements. Diffraction patterns of hydrating strontium aluminate revealed rapid dissolution of the anhydrous parent phase, evidenced by a pronounced drop in the intensity of its primary reflection at 28.381 degrees two-theta within the first thirty to sixty minutes after water addition. The newly formed hydration products remained amorphous throughout the initial twenty-four hours of curing, after which distinct diffraction peaks corresponding to cubic hexahydrate crystalline phases emerged, marked by a primary reflection at 16.651 degrees two-theta. Aluminum-27 magic-angle spinning nuclear magnetic resonance spectra corroborated this structural reorganization. The unhydrated cement exhibited a dominant resonance near 65 parts per million corresponding to tetrahedrally coordinated aluminum units within corner-sharing networks, whereas hydrated samples displayed a distinct resonance near 10 parts per million within three hours of mixing, signaling the progressive formation of octahedrally coordinated aluminum species in the developing amorphous gel.

Time-resolved micro-Raman spectroscopy provided additional spatial and vibrational evidence of the rapid interfacial breakdown. Group theory predicts eighty-one Raman-active optical modes for monoclinic strontium monoaluminate, though individual grains experimentally exhibited a discrete subset of sharp bands. Sequential Raman spectral mapping revealed non-uniform grains embedded in an aqueous matrix, showing progressive particle shrinkage and fragmentation accompanied by the attenuation of the prominent 465 reciprocal centimeter bending vibration associated with corner-sharing aluminum-oxygen tetrahedra. Between twenty and four hundred fifteen minutes of hydration, a broad spectral band above 3000 reciprocal centimeters associated with free pore water steadily declined, while a sharp hydroxyl vibration emerged at 3600 to 3650 reciprocal centimeters after approximately ninety minutes. This early hydroxyl feature revealed the local structural assembly of poorly crystalline or amorphous hydrated strontium aluminate structures well before long-range crystalline ordering became detectable by powder X-ray diffraction.

Isothermal conduction calorimetry performed at 20 degrees Celsius highlighted fundamental differences in heat evolution and reaction kinetics between the two cement systems. Strontium aluminate paste generated an immediate, intense exotherm upon contact with water, producing an initial calorimetric peak within twenty minutes that reflected rapid wetting, clinker dissolution, and early precipitate nucleation without any measurable dormant period. A broader secondary exothermic peak spanned from one to thirty hours as dissolved aluminate and strontium species reacted to form the solid gel matrix, after which the system transitioned into a diffusion-controlled regime characterized by decreasing heat output. Conversely, ordinary Portland cement exhibited a sharp initial wetting peak at three minutes that was approximately eight times more intense, followed by a well-defined induction or dormant stage lasting from thirty minutes to four hours. Accelerated reaction commenced only after five hours, followed by deceleration after twenty hours and diffusion control beyond forty hours.

In-situ luminescence confocal microscopy and intensity tracking over the initial two and a half hours demonstrated how the spatial distribution of nanodiamonds reflects early hydration stages. When water was introduced, nanodiamonds were initially dispersed through the pore solution, producing a modest initial surge in luminescence before adsorbing onto grain surfaces as dissolution proceeded. As the amorphous gel precipitated, it progressively encapsulated the diamond nanoparticles, stabilizing them against unrestricted Brownian motion and leading to gradual luminescence quenching through radiation reabsorption by the growing solid phases. In the terbium-doped strontium aluminate paste, this quenching process proceeded rapidly during the first hour before plateauing as diffusion barriers formed. In contrast, ordinary Portland cement showed a much slower, gradual reduction in nanodiamond luminescence intensity, mirroring its prolonged dormant interval and delayed microstructural consolidation.

Direct optically detected magnetic resonance spectra collected across the initial hours confirmed that quantum defect spins accurately track these chemical kinetics. The measured zero-field splitting resonance for strontium aluminate paste appeared at 2.86977 gigahertz, compared to 2.869803 gigahertz in ordinary Portland cement and 2.868758 gigahertz in pure aqueous nanodiamond suspensions. The resonance frequency exhibited a split profile reflecting hyperfine coupling to the nitrogen-14 nuclear spin, while the total resonance linewidth underwent dramatic three-stage evolution. In the strontium aluminate paste, linewidth reached an initial maximum within twenty minutes of wetting, contracted to a minimum near sixty minutes as dissolution gave way to intense chemical bonding, and stabilized after approximately three hours. By tracking thermal frequency shifts, the authors determined that local hydration-induced temperature increases during the first hour reached approximately 1.2 degrees Celsius in strontium aluminate paste and 11.0 degrees Celsius in Portland cement paste. Allan deviation analyses demonstrated high frequency stability down to 20 kilohertz before long-term thermal drift intervened beyond 100,000 seconds.

Time-resolved longitudinal spin relaxometry further clarified the microscopic interfacial environment by quantifying the spin-lattice relaxation time of the defect centers. During the initial hydration phase, rapid dissolution and ionic release into the surrounding pore solution generated substantial local magnetic and electric field fluctuations, reducing the relaxation time of the defect spins. In the strontium aluminate binder, spin relaxation times evolved rapidly during early wetting and ion dissolution, approaching a stable plateau after eight hours that coincided with the calorimetric deceleration boundary and the onset of diffusion-controlled transport. Ordinary Portland cement displayed a considerably delayed response, with successive relaxation maxima appearing substantially later in accordance with its prolonged induction kinetics. By demonstrating that internal rare-earth dopants can directly drive quantum defects to monitor early hydration, the authors have established an experimental framework for characterizing reactive ceramic binders intended for terrestrial engineering and extreme extraterrestrial environments.

Subject of Research: Direct optically detected magnetic resonance tracking of cement hydration dynamics using nitrogen-vacancy centers and terbium luminescence

Article Title: Tracing Tb-SrAl2O4 hydration dynamics through Tb–NV− interactions using direct optically detected magnetic resonance (dODMR)

Article References: Kruk, A., Mrózek, M., Kreiβl, S., & Madej, D. (2026). Tracing Tb-SrAl2O4 hydration dynamics through Tb–NV− interactions using direct optically detected magnetic resonance (dODMR). Archives of Civil and Mechanical Engineering, 27(1), Article 6. https://doi.org/10.1007/s43452-026-01680-6

Image Credits: AI Generated

DOI: 10.1007/s43452-026-01680-6

Keywords: Strontium Aluminate, Optically Detected Magnetic Resonance, Nitrogen-Vacancy Centers, Nanodiamonds, Terbium Doping, Cement Hydration, Ordinary Portland Cement, Spin Relaxation, Isothermal Calorimetry, Raman Spectroscopy, Nuclear Magnetic Resonance, X-ray Diffraction, Microstructural Evolution, Quantum Sensing, Space Materials, Radiation Shielding